Flux Core Welding Settings Chart by Wire Diameter
A flux core welding settings chart matches wire diameter to steel thickness and gives voltage and wire speed starting points to dial in on scrap before the real weld.

On this page
Top picks at a glance
As an Amazon Associate I earn from qualifying purchases.
- 1
ARCCAPTAIN Flux Core Welding Wire E71T-GS .035" 2LB x 39.5/10View on Amazon - 2
Handheld Welder9.4/10View on Amazon
A gate hinge has cracked off its post, and the repair has to hold out in the wind with no gas cylinder on hand. A flux core welding settings chart is the starting point for that weld: it matches wire diameter to the steel in front of you, then points to a voltage and wire speed range to dial in from. This guide shows how to read that chart, what each setting does, and how to check the result on scrap before welding the real joint.
This guide links to our product roundups, where WeldGearLab gets a commission on purchases made through links on this page, and your price stays the same. Read our affiliate disclosure.
What a flux core welding settings chart tells you
A settings chart is a table, not a rule. It is usually organised by steel thickness and wire diameter, and each cell gives a voltage and wire speed starting point. Learn what flux core wire is and how the flux inside it shields the puddle, and the chart starts to make sense.
The chart on the inside of the machine door is usually the best starting point, because it matches the machine in front of you. A printed chart in a wire box or in a guide is a starting point, not a setting to weld blind from.
Side by side
| .030 inch wire | .035 inch wire | What to check | |
|---|---|---|---|
| Wire types listed | E71T-GS and E71T-11 | E71T-GS | Match the classification on the spool label |
| Spool weights listed | 2 lb | 2 lb and 10 lb | Heavier spools suit longer runs of welding |
| Shielding gas | None, self-shielded | None, self-shielded | Flux inside the wire shields the puddle |
| Polarity listed | DCEN for E71T-11 | Follow the wire label | Check the label and the machine manual |
| Outdoor use | Suited to wind and drafts | Suited to wind and drafts | Flux core tolerates a breeze better than gas |
The table above shows what the listings behind this guide state. The .030 inch listings cover E71T-GS and E71T-11 wire, while the .035 inch listings cover E71T-GS. Spool weights run from 2 lb rolls up to 10 lb spools. Blue Demon lists DCEN for its E71T-11 wire, and other listings leave polarity unstated, so follow the wire label and the machine manual.
How to read the chart step by step
Work through the chart in order.
- Find the wire diameter on the spool label: .030 inch or .035 inch in the listings behind this guide.
- Find the steel thickness row. Match the row to the steel in front of you.
- Read across to voltage and wire speed: those are starting points, not finished settings.
- Check polarity. E71T-11 wire in the listings runs on DCEN; set the polarity the wire label calls for.
- Weld on scrap of the same thickness, chip the slag, and look at the bead before touching the real joint.
- Adjust from what you see. A stubbing arc wants more voltage or less wire speed; a long, spattery arc wants the reverse.
If the bead looks right on scrap and the slag chips off clean, the settings are close enough to weld the joint. If not, check polarity, stickout, and whether the steel is clean enough for the wire to wet in.
Wire diameter sets the range
Wire diameter helps set the range of steel a setup can cover. The listings behind this guide stock .030 inch and .035 inch flux core wire, and those sizes cover most home, farm and hobby work. Thinner wire suits thin steel, where less heat is wanted; thicker wire carries more metal into the joint and suits heavier steel.
ARCCAPTAIN lists its .035 inch E71T-GS wire in 2 lb spools, sold as a pack with a net weight of 6 lb. Rumvita and KISWEL list .035 inch E71T-GS wire on 10 lb spools. YixangDD lists .030 inch E71T-GS wire in 2 lb rolls, and Blue Demon lists a .030 inch E71T-11 spool at 2 lb in the title, though the spec table lists 1.8 pounds. When a listing disagrees with itself, treat the weight as approximate and check with the seller. See the best flux core wire .030 and best .035 flux core welding wire roundups.
Voltage and wire speed work together
Voltage sets the arc length and the heat in the puddle. Wire speed sets how fast wire feeds into the puddle, which sets the amperage the arc draws. Turn the voltage up and the arc gets longer and hotter; turn the wire speed up and more metal feeds in. The chart lists them together because changing a setting on its own moves the weld out of balance.
A stubbing wire wants more voltage or less wire speed. A long arc that spatters and hisses wants less voltage or more wire speed. Make a change, weld a bead on scrap, and read the bead before changing anything else. The MIG welder wire speed and voltage chart covers the same settings for solid wire.
Dial in on scrap before the real joint
Scrap of the same thickness as the joint is the best practice there is. Weld a straight bead, let it cool enough to handle, chip the slag, and look at the bead: even edges, a steady width, and slag that lifts off clean mean the settings are close. A narrow, tall bead wants more heat; a wide, flat bead with undercut at the edges wants less.
Keep the gun angle and the travel speed steady while dialling in, so a change in the bead comes from the setting and not from the hand. If the bead changes when the settings stay put, check the wire feed: a slipping drive roll or a kinked liner shows up as an uneven arc. See MIG welder set up before welding.
What to check before you weld
- Polarity. Set the polarity the wire label calls for. E71T-11 wire in the listings runs on DCEN.
- Drive rolls. Flux core wire wants knurled drive rolls that grip without crushing the hollow wire.
- Stickout. Keep stickout steady, and keep the contact tip in good shape.
- Steel prep. Flux core tolerates rust and mill scale better than solid wire, but heavy rust, paint and oil still need cleaning off the joint.
- Ventilation and cover. Flux core makes more smoke than gas MIG, so weld outdoors or with the shop door open and the head out of the plume.
Flux core smoke and slag. Flux core makes more smoke and fumes than gas MIG, and hot slag can flick off when chipped. Weld with good ventilation or outdoors with the head out of the plume, and wear safety glasses under the helmet when chipping. See the flux core welding pros and cons guide.
For more options, see our welders guides.
FAQ for welders
What wire diameter should a beginner start with for flux core welding?
Start with the diameter the chart row calls for, and with what the machine supports. The listings behind this guide stock .030 inch and .035 inch wire: .030 inch suits thin steel and small machines, while .035 inch is the common all-round size for home and farm work.
What does wire speed do on a flux core welder?
Wire speed sets how fast wire feeds into the puddle, which sets the amperage the arc draws. More wire speed feeds more metal and raises the heat; less wire speed feeds less metal and lowers it. If the wire stubs, raise the voltage or lower the wire speed; if the arc gets long and spattery, do the reverse.
Why does a flux core weld spatter so much?
Spatter comes from an arc that is too long, a voltage that is too high for the wire speed, or dirty steel. Shorten the arc by lowering the voltage or raising the wire speed, and clean heavy rust, paint and oil off the joint. Some spatter is normal with flux core.
Does flux core wire need gas?
No. Self-shielded flux core wire, such as the E71T-GS and E71T-11 wire in the listings behind this guide, carries flux inside the wire that burns to make its own shielding gas. That is why flux core works outdoors in a breeze where gas shielding blows away. Gas-shielded flux core wire is a separate type that does need gas, so check the classification on the spool. See gasless vs gas shielded flux core wire for the full split.
Can the same settings chart cover E71T-GS and E71T-11?
Use the chart as a starting point for each wire, and dial in on scrap before welding the joint. E71T-GS in the listings is described as all-position and suited to single-pass and multi-pass welding, while the E71T-11 listing describes it as designed for multi-pass work and running on DCEN. Treat each spool as its own starting point and check the label.
Related: what flux core wire is, best flux core welder, MIG welder wire speed and voltage chart, and flux core vs MIG. Also see the how to choose a MIG welder guide.