TIG Welding Problems and Solutions: Common Defects and Shop Fixes
Troubleshoot common TIG welding problems including porosity, tungsten contamination, arc wander, and cracking with direct bench solutions that clean up your bead.

On this page
You strike an arc on clean steel or aluminum tubing on the shop bench, add filler rod, and watch the puddle foam with black crust, wander away from the joint, or blow a hole right through the metal. Most tig welding problems and solutions come down to shielding gas coverage, tungsten preparation, heat control, and joint cleanliness. Solving them at the bench means isolating whether the defect comes from atmospheric contamination, an improper arc gap, or dirty base metal before changing machine settings.
As an Amazon Associate I earn from qualifying purchases. This guide links to our product roundups, where WeldGearLab gets a commission on purchases made through links on this page, and your price stays the same. Read our affiliate disclosure.
TIG welding problems and solutions in one paragraph
TIG welding relies on pure shielding gas, clean base metal, and a steady hand. Because the tungsten electrode never touches the work, any contact with the puddle, filler rod, or surface scale contaminates the tip and creates an erratic arc. Similarly, any shop draft or loose torch fitting draws in outside air that turns the bead dark and leaves porosity holes in the joint. Keep the tungsten ground along its axis, clean the joint with a dedicated stainless wire brush, hold a close arc gap, and maintain post-flow gas until the puddle cools.
Side by side troubleshooting guide
| Defect | Visual Sign | Likely Cause | Shop Fix |
|---|---|---|---|
| Porosity | Pinholes and bubbling pockets across the bead | Drafts blowing gas, dirty base metal, or lack of post-flow | Shield the torch, clean the joint with acetone, and maintain post-flow |
| Tungsten contamination | Black specks in bead and erratic fluttering arc | Dipping tungsten into puddle or touching filler rod to tip | Stop immediately, break the dirty tip, and grind longitudinally |
| Arc wandering | Arc dances around joint instead of rooting in puddle | Radial grinding marks, long arc gap, or dirty ground contact | Grind taper along electrode axis, tighten arc gap, and clean ground clamp |
| Burn-through | Holes blown through sheet and excessive root sag | Slow travel speed, excessive heat input, or tight joint fit-up gap | Speed up travel, taper amperage on the pedal, and use aluminum backing |
| Crater cracking | Star-shaped fissure in bead termination crater | Abrupt arc termination and releasing pedal too quickly | Taper current down slowly and add a final dab of filler rod |
| Bead oxidation | Black, gray, or crusty discoloration on stainless | Inadequate gas shielding coverage or excessive heat on stainless | Use a gas lens with larger cup, maintain gas coverage, and increase travel speed |
| Torch instability | Shaky filler feed and accidental puddle dipping | Fatigue, lack of wrist support, or stiff heavy gloves | Rest wrist on a prop, relax grip, and wear goatskin gloves with a 4-inch cuff |
Settings and technique depend on base metal thickness and joint fit-up; always check your machine door chart and manual before adjusting arc balance or amperage. Good torch control starts with a comfortable hand position and clear sightlines through your hood.
Porosity and shielding gas contamination
Porosity happens when atmospheric oxygen and nitrogen enter the molten puddle, leaving clusters of pinholes or bubbling swiss-cheese pockets across the bead. In almost every case, porosity indicates a breakdown in shielding gas coverage rather than a machine fault.
- Drafts and air movement. Even a light breeze from an open shop door or a cooling fan blows away argon shielding gas. Set up welding screens around your bench to block drafts completely.
- Torch hardware leaks. Check the back cap O-ring, collet body, and gas lens. A cracked O-ring draws outside air directly into the gas stream through venturi suction. Tighten all torch components snugly by hand.
- Dirty base metal and filler rod. TIG requires immaculate metal. Mill scale, rust, cutting oil, and moisture boil into gas when heated. Grind the joint to bare metal, wipe it down with acetone, and wipe filler rods clean before striking an arc.
- Premature torch pull-away. Moving the torch away immediately after breaking the arc exposes hot metal to atmosphere. Hold the torch cup stationary over the puddle until post-flow argon stops flowing.
For setup details on gas flow, see our guide to TIG welding argon flow rate and learn why shielding failures explain why are my TIG welds black.
Tungsten contamination and arc wander
An erratic arc that dances around the joint or jumps from side to side prevents clean puddle control. This problem almost always traces back to a fouled electrode or incorrect grinding technique.
- Dipping into the puddle. Touching the tungsten electrode into the molten puddle or bumping it with the filler rod deposits metal onto the tip. This alters arc shape and sends tungsten inclusions into the weld. Stop immediately, break off the fouled tip, and regrind the point.
- Radial grinding marks. Grinding a tungsten across the wheel leaves circular scratches that encourage the arc to spin and wander. Always grind longitudinally so scratch lines run parallel along the electrode length toward the tip.
- Poor work clamp contact. A loose ground clamp or one attached over rust, mill scale, or paint disrupts electrical flow. Attach the clamp directly to clean bare metal as close to the joint as possible.
Read our guide on how to sharpen tungsten for TIG welding and review electrode selection in what color tungsten for steel.
Burn-through and excessive heat input
Burning through thin sheet metal, excessive sag on the root side, and severe workpiece warping indicate that too much heat is soaking into the part faster than it can dissipate.
- Slow travel speed. Lingering in one spot overheats the base metal. Maintain a brisk, steady travel speed and add filler wire consistently to cool the puddle.
- Excessive amperage. Running higher current than necessary causes the puddle to expand uncontrollably. Ease off the foot pedal as the workpiece heats up during long passes.
- Wide arc length. Long-arcing increases voltage and spreads heat over a wider surface area. Keep the tungsten tip close to the puddle without touching.
- Poor heat sinking. Thin metal needs help shedding heat. Clamp heavy aluminum or copper backing bars behind the joint to draw thermal energy away from the weld zone.
For specialized techniques on thin stock, review our guide to how to TIG weld thin stainless without warping.
Crater cracking and poor puddle termination
Crater cracks form at the very end of a bead, often spreading outward in a star pattern. These shrinkage cracks occur when the arc is cut abruptly while the puddle remains molten.
- Sudden arc stop. Releasing the foot pedal instantly leaves a concave, hot crater that pulls apart under thermal stress. Ease off the pedal gradually to taper current down smoothly.
- Starved weld crater. Ending a weld without adding filler leaves the center of the bead thin and prone to cracking. Add a final dab of filler rod into the crater while tapering off the amperage.
- Short post-flow duration. Shielding gas must continue flowing until the solidifying crater drops below oxidation temperature. Keep your post-flow active and hold the torch cup steady over the terminated bead.
For filler selection across common metals, browse our guide to the best TIG rod for mild steel and our guide to the best TIG rod for stainless steel.
Torch control, hand stability, and safety gear
Torch control issues often stem from hand fatigue, an unsteady rest position, or restrictive safety gear. Because TIG welding generates minimal spatter compared to MIG or stick, gloves designed specifically for TIG prioritize dexterity and tactile sensitivity over heavy thermal padding.
Gloves with thick cowhide palms make feeding thin filler wire awkward and cause welders to squeeze the torch tightly, resulting in hand cramps and accidental tungsten dips. Tillman lists a 4-inch cuff on its 1338 pearl top grain goatskin gloves, combining wrist protection against radiant heat with an unlined palm for precise filler rod control. Caiman specifies a 4-inch extended cuff with an ANSI/ISEA Heat Level 2 rating on its 1540 goatskin model, along with Kevlar stitching and a 30-day warranty. Defiant Metal lists premium black goatskin gloves with an unlined palm and a 14-day warranty on manufacturer defects, while Tillman provides an 11-inch glove length on its 1488 TrueFit model with Kevlar stretch inserts. Pair quality gloves with a stable wrist rest on the bench to support your torch hand, allowing your fingers to glide freely along the seam.
TIG arcs emit intense ultraviolet radiation that reflects off surrounding metal and causes rapid arc flash burns. Wear flame-retardant clothing, leather sleeves, and high-top leather work boots. Anchor argon cylinders upright with a chain, and maintain adequate shop ventilation to prevent shielding gas from displacing oxygen in enclosed spaces. Check our scored recommendations in the best welding gloves for dexterity, inspect our top picks in the best welding helmet for TIG welding, and browse our complete welding safety gear section. Read our Safety Disclaimer.
FAQ for welders
Why does my TIG tungsten keep turning black?
Tungsten turns black when atmospheric air reaches the hot electrode before shielding gas can protect it. This happens when the welder pulls the torch away before post-flow gas stops, when shop drafts blow argon away, or when torch fittings leak. Inspect the torch back cap O-ring, maintain gas shielding until cooling finishes, and verify that gas hardware remains tight.
What causes pinholes and porosity in TIG welds?
Porosity occurs when air enters the molten weld pool and leaves voids as the metal solidifies. Common causes include oil, rust, or moisture on the metal, dirty filler rod, shop drafts, or a damaged gas lens. Clean base metal thoroughly with a stainless wire brush, wipe joints with acetone, and block breezes around your bench.
Why does my TIG arc wander and fail to start smoothly?
An erratic arc usually stems from radial grinding marks, a contaminated electrode tip, or poor electrical contact at the work clamp. Grinding across the tungsten creates circular ridges that force the arc to dance. Grind longitudinally along the electrode axis toward the point, maintain a close arc gap, and attach your ground clamp directly to clean bare metal.
How do I stop crater cracking at the end of a TIG bead?
Crater cracks occur when you terminate the arc abruptly, leaving a thin crater that splits as it contracts. Gradually taper down amperage using your foot pedal while adding a final dab of filler rod to crown the crater. Keep the torch in place over the puddle until post-flow argon ceases.
Can the wrong welding gloves cause TIG welding defects?
Heavy or stiff gloves reduce tactile sensitivity, making it difficult to feed filler wire smoothly and control torch height. Welders often dip the tungsten when hand fatigue sets in or when bulky cuffs catch on the table. Thin goatskin gloves provide the finger flexibility needed for delicate filler control while protecting hands from radiant heat.
Related: best entry level TIG welder, best TIG torch, best welding gloves for dexterity, and the TIG welders hub. Also see our guide on what shade lens for TIG welding.