Flux Core Welding Problems and How to Fix Them

Spatter, porosity, slag, burn-through and wire feed faults are the common flux core welding problems, and each one points to a cause you can check before the next pass.

Flux Core Welding Problems and How to Fix Them
On this page

Top picks at a glance

As an Amazon Associate I earn from qualifying purchases.

  1. 1DURATECH 125A MIG WelderDURATECH 125A MIG Welder9.7/10View on Amazon
  2. 2YESWELDER 135A MIG WelderYESWELDER 135A MIG Welder9.6/10View on Amazon
  3. 3ARCCAPTAIN Flux Core Welding Wire E71T-GS .035" 2LB x 3ARCCAPTAIN Flux Core Welding Wire E71T-GS .035" 2LB x 39.5/10View on Amazon

A bead that looks like popcorn, a weld full of holes, slag that will not come off: flux core welding problems usually trace back to a small set of causes, and most of them show up in the bead before they show up anywhere else. Flux core welding problems come from the wire, the polarity, the stickout, the travel speed and the metal itself, and this guide walks through each one and what to check first.

This guide links to our product roundups, where WeldGearLab gets a commission on purchases made through links on this page, and your price stays the same. Read our affiliate disclosure.

Flux core welding problems at a glance

Problem What it looks like Likely cause Check first
Too much spatter Balls of metal stuck around the weld Wrong polarity or wire speed Polarity on the wire label, then wire speed
Porosity Pinholes in the bead Damp wire, draft or dirty metal Dry wire, clean joint, shelter from wind
Slag inclusions Slag trapped inside the weld Welding over slag from the last pass Chip and brush between passes
Burn-through Holes melted through thin metal Too much heat or slow travel Lower heat, faster travel, tighter fit
Wire jams Wire tangles at the drive rolls Drive roll tension, liner or tip Drive rolls, liner, tip size for .035 wire
Lack of fusion Bead sits on top without tying in Too cold or too fast Heat setting, travel speed, clean joint
Rough, ropey bead Uneven bead with a poor profile Long stickout or wrong gun angle Stickout, gun angle, travel speed
Excess smoke Heavy smoke from the arc Flux burning off Ventilation, head out of the plume

Polarity and settings follow the wire label and the machine manual. The checks below start with the wire and the setup, not the welder.

Too much spatter

Spatter is the shower of small balls of molten metal that stick to the work around the weld. It wastes wire, and it costs time with a grinder after the weld cools. The first thing to check is polarity: self shielded flux core wire usually runs with the electrode negative, often marked DCEN, and running it the other way makes the arc harsh and the spatter worse. Follow the polarity printed on the wire label and in the machine manual.

After polarity, look at wire speed and stickout. Wire speed set too high for the voltage pushes more metal into the arc than the arc can melt cleanly, and a long stickout makes the arc wander. Both reference wires for this guide are E71T-GS in .035 inch, and the makers list them as low spatter wire: Rumvita lists its E71T-GS .035 inch wire as low spatter with little to zero post-weld cleanup, and KISWEL lists low spatter generation for its E-71TGS .035 inch wire. If a wire that claims low spatter still throws spatter everywhere, the setup is the place to look, not the spool.

Porosity: holes in the bead

Porosity shows up as pinholes or small round holes in the bead, and it weakens the weld because the holes are voids where metal should be. Gas gets trapped in the puddle as it freezes, and the usual sources are damp wire, a draft across the arc, or dirt on the joint. Self shielded flux core wire handles outdoor and drafty work better than gas MIG, and Rumvita lists its wire for welding outdoors or in drafty conditions.

Keep the wire dry. Rumvita vacuum packs its wire to keep it waterproof, moistureproof and dustproof, which is the right idea for any spool: a spool left open in a damp shop picks up moisture, and damp flux makes porous welds. Shield the arc from wind and clean the joint before welding.

Slag inclusions and slag that will not come off

Slag is the crust the flux leaves on the bead, and some slag is normal with flux core wire. The problem starts when slag gets trapped inside the weld instead of sitting on top. That happens when a pass is laid over slag left from the pass before it, so the slag ends up buried between layers where no hammer can reach it.

Chip and brush between every pass. A chipping hammer and a wire brush take a minute per pass, and they are the usual way to be sure the next pass fuses to clean metal. KISWEL lists easy slag removal for its wire, which helps here, but no wire lets you skip the cleaning step.

Burn-through on thin metal

Burn-through is a hole melted clean through the work, and it shows up most on thin sheet and at the edge of a joint. The cause is heat the metal cannot carry away: too much heat for the thickness, travel too slow, or a gap that lets the arc blow straight through. The fix is to put less heat into the joint: lower the heat, move faster, and close the gap with a tighter fit-up before striking an arc.

Stitch welding helps on thin panels: short beads with a pause between them let the metal cool, instead of a long bead that pours heat into a small area. Tack the joint well first to hold the fit as the metal heats.

Wire feed problems: jams and bird-nesting

Bird-nesting is the tangle of wire that piles up at the drive rolls when the wire stops moving through the liner but the rolls keep feeding. The wire has to go somewhere, so it coils into a nest inside the machine. The usual causes are drive roll tension set wrong, a worn or kinked liner, a contact tip that does not match the wire, or a spool that does not turn freely.

Check the drive rolls first. Too little tension lets the wire slip, and too much tension flattens the wire and jams it in the liner. The tip size must match the wire: both reference wires here are .035 inch, so the tip, the liner and the drive rolls all need to suit .035 inch wire. The spool should turn freely on its hub without overrunning.

Lack of fusion and cold lap

Lack of fusion means the bead sits on top of the metal without tying into it, and cold lap is the same fault at the edge of the bead, where the metal rolls over without fusing to the base. The weld looks laid on rather than melted in, and it can break along the joint under load. The causes are a bead run too cold, travel too fast, or a dirty joint that keeps the puddle from wetting into the metal.

Watch the puddle, not the arc. The puddle should wash into both sides of the joint, with the edges melting and flowing together. If the bead stands tall and narrow with a sharp edge, add heat or slow down until the puddle ties in. Clean the joint first, since mill scale, rust and paint all block fusion.

Excess smoke and fumes

Flux core makes more smoke than gas MIG, because the flux burns off as the wire melts. The smoke carries fume from the flux and the metal, and it needs to leave the breathing zone. Weld with good ventilation, or outdoors with your head out of the plume.

Clear the area of anything flammable before striking an arc, since spatter and hot slag travel further than most welders expect. Wear safety glasses under the helmet when chipping slag. Galvanized steel needs extra care: the zinc coating makes heavy fume, so grind the coating off the joint and weld with strong ventilation.

Which wire to run

Both reference wires for this guide are E71T-GS in .035 inch on 10 lb spools, which is a common home shop size for flux core work. Rumvita lists its wire as copper-coated mild steel for single or multi-pass welds, self shielded with no need for external gas or flux, and vacuum packed. KISWEL lists its wire as made in the USA, for all-position welding with open-arc transfer, low spatter generation, easy slag removal.

Match the wire to the machine. Check the machine manual for the wire diameters it supports, and match the drive rolls, liner and contact tip to the wire in the machine. The flux core welding wire sizes guide covers diameter choice, and the flux core welding wire types guide covers gasless and gas-shielded wire. See the flux core welding settings chart for settings by diameter.

FAQ for welders

Why does my flux core weld spatter so much?

Check polarity first, since self shielded flux core wire usually runs electrode negative and the wrong polarity makes spatter worse. Then check wire speed, stickout and joint cleanliness. A wire that lists low spatter still throws spatter when the setup is off.

Why is my flux core weld full of holes?

Holes in the bead are porosity, usually from damp wire, a draft across the arc, or a dirty joint. Keep the spool dry, clean the metal, and shield the arc from wind.

Do I need gas with flux core wire?

No. Self shielded flux core wire like E71T-GS makes its own shielding gas from the flux as it burns, so it needs no cylinder, hose or regulator. That is why it suits outdoor and drafty work, where gas from a cylinder would blow away.

What polarity does flux core wire use?

Self shielded flux core wire usually runs DCEN, electrode negative, but always follow the polarity printed on the wire label and in the machine manual. The label is the authority for that spool, and some wires differ.

Can flux core wire weld outdoors?

Yes. Self shielded wire needs no external gas, so wind does not strip the shielding the way it does with gas MIG. Rumvita lists its E71T-GS wire for welding outdoors or in drafty conditions.

Related: how to choose a MIG welder, best flux core welder, best welder for beginners, the MIG welders hub, and the main welders hub. Also see the flux core welding setup guide and flux core wire welding tips.

More buying guides

Welders ·

Flux Core Welding Setup for Beginners

Flux core welding setup, step by step: power, wire, polarity and feed speed for a gasless 120V welder, with the figures from 3 reference…